Is Ripstop Fabric Tear-Proof? What Buyers Should Test

Ripstop grids do not guarantee tear resistance. Learn how yarns, PU coating, and test methods affected a real lightweight-jacket fabric project.

FABRIC TESTING

CC Textile

11/28/20267 min read

Visitors at a textile trade show
Visitors at a textile trade show

Ripstop fabric is not tear-proof. Its reinforced grid can help slow a small tear, but the final result depends on the yarns, construction, density, weight, finishing process, and test method.

A CC Textile lightweight-jacket project showed why the distinction matters. The fabric was a 50D, 100% polyester ripstop with a PU coating and a finished weight of approximately 87 GSM. Although the grid was clearly visible, the coated fabric failed the customer’s tear-strength requirement.

What Does Ripstop Fabric Actually Do?

Ripstop is a woven construction with reinforcement yarns at regular intervals, creating a square or rectangular grid.

The reinforced yarns may restrict a tear once damage starts. That balance of low weight and resistance to tear propagation makes nylon and polyester ripstop relevant to lightweight jackets, windbreakers, outdoor pants, and bags.

The grid is one part of the specification. Tear performance also depends on:

  • Fiber composition

  • Yarn denier

  • Yarn strength and grade

  • Warp and weft density

  • Size and spacing of the reinforced grid

  • Fabric weight

  • Weaving quality

  • Dyeing and heat treatment

  • Coating or lamination

  • Direction and method of tear testing

“50D polyester ripstop” is therefore an incomplete specification. Fabrics with that same description can produce different tear-test results.

Why Can Ripstop Fabric Still Tear?

The reinforcement grid cannot compensate for every weakness in the base cloth or finish. Tear-test failures can occur when:

  • The base yarn is not strong enough for the target use.

  • The warp or weft density is too low.

  • The reinforced grid is too widely spaced.

  • The construction is unbalanced between warp and weft.

  • The finished fabric has become too stiff or brittle.

  • A coating restricts yarn movement at the tear point.

  • The test requirement is higher than the construction was designed to meet.

  • The submitted sample and bulk fabric do not follow the same processing route.

Tear location and direction matter. Warp and weft can behave differently because their yarn specifications or densities may differ. Request results in both directions when required by the garment specification.

A 50D Polyester PU-Coated Ripstop That Failed

The lightweight-jacket project used the following specification:

  • Composition: 100% polyester

  • Yarn specification: 50D

  • Construction: ripstop

  • Finish: PU coating

  • Weight: approximately 87 GSM

  • Intended use: lightweight jacket

  • Testing stage: after PU coating

The final coated fabric fell below the customer’s minimum tear strength. The exact values and customer-appointed method are not disclosed, so this case cannot be compared numerically with results from a different test method.

Testing took place after PU coating. A test on the uncoated base cloth alone would not have shown how the complete finishing process affected tear strength.

How PU Coating Can Affect Tear Strength

PU coating can modify a fabric’s surface, hand feel, or resistance to water penetration. Its effect depends on the formulation, application amount, curing conditions, and compatibility with the base cloth.

Coating does not automatically reduce tear strength. During tearing, yarns may move and gather to redistribute the force. An unsuitable coating can restrict that movement or make a lightweight structure stiff or brittle, reducing its tear resistance under the selected test conditions.

In this project, the original PU coating process made the lightweight polyester ripstop too brittle, and the final tear result fell below the customer’s minimum. This was a problem with that combination of base cloth, coating, and processing conditions—not evidence that all PU-coated ripstop is weak.

How the Coating Process Was Corrected

The team reviewed the coating process instead of simply increasing fabric weight or adding a heavier grid. Three areas were adjusted:

  • Coating formulation

  • Processing parameters

  • Processing temperature

After those adjustments, the finished fabric was retested and achieved tear strength slightly above the customer’s minimum. The result showed that the coating process was as important to approval as the visible ripstop structure.

A result just above the minimum leaves little allowance for normal production variation. Agree on an appropriate performance margin with the buyer, supplier, and testing laboratory before bulk production.

Tear Strength Is Not the Same as Tensile Strength

Tear strength measures resistance to the continuation of an existing cut or tear. Depending on the method, testing may use a falling pendulum, a tongue-shaped specimen, or a trapezoid specimen.

For example, ASTM D1424 measures the force needed to propagate a single-rip tear with a falling-pendulum apparatus. Its results should not be treated as interchangeable with results from other tear methods.

Tensile testing measures how the fabric responds to pulling, including its breaking force or behavior at a specified test condition.

A tear-strength specification should state:

  • Test method

  • Test direction

  • Unit of measurement

  • Minimum warp requirement

  • Minimum weft requirement

  • Sample conditioning

  • Whether the fabric is tested before or after finishing

“High tear strength” gives the mill, coating processor, and laboratory no measurable acceptance criterion.

Tear Strength, Abrasion and DWR Measure Different Risks

A lightweight outdoor jacket may need several tests because tear strength, abrasion resistance, and surface water repellency address different risks.

Tear strength: This checks how the fabric resists the propagation of existing damage. A ripstop grid is directly relevant, but the complete coated construction still determines the result.

Abrasion resistance: This evaluates how the fabric responds to repeated surface rubbing. The customer’s requirement in this project was 16,000 abrasion cycles.

The 16,000-cycle target also needs a method, abrasive material, pressure or load, evaluation endpoint, and pass criteria. The same cycle count under another method may represent a different level of abrasion.

Water repellency: The project used an AATCC 22 initial requirement of 90 or above. AATCC TM22 evaluates a fabric’s resistance to surface wetting by water and is particularly suitable for assessing water-repellent finishes.

An AATCC 22 spray rating does not establish waterproofness. If resistance to water penetration is required, specify a separate hydrostatic-pressure method and acceptance level.

Passing one of these tests does not establish performance in the others. A fabric can pass its initial spray test and fail tear testing, or meet tear and abrasion requirements without meeting a waterproof specification.

Is PU-Coated Ripstop Waterproof?

PU-coated ripstop can be developed to resist water penetration, but “PU coated” alone is not a measurable waterproof specification.

Performance depends on factors including:

  • Coating type and application amount

  • Coating continuity

  • Base fabric construction

  • Pinholes or coating defects

  • Required hydrostatic pressure

  • Washing or aging conditions

  • Garment seams and construction

For a waterproof lightweight jacket, state the hydrostatic-head target and method in the RFQ. Keep AATCC 22 as a separate surface-repellency requirement.

This distinction is covered further in our guide to waterproof fabric specifications.

Is Nylon or Polyester Ripstop Better for Jackets?

Both nylon and polyester ripstop can work for lightweight jackets. The appropriate choice depends on the garment, hand feel, weight, strength, color, finishing process, and cost target.

Fiber name alone does not predict tear performance. A suitable polyester construction may outperform an unsuitable nylon one, while a different nylon fabric may be the better choice for another garment. Compare finished specifications and test results.

Useful comparison points include:

  • Denier

  • GSM

  • Warp and weft density

  • Tear strength in both directions

  • Abrasion resistance

  • Hand feel and noise

  • Coating or lamination

  • Water-repellency requirement

  • Hydrostatic pressure where applicable

  • Packability

  • Bulk consistency

CC Textile’s woven fabric catalog includes different performance and ripstop constructions, but a listed product should still be evaluated against the intended garment requirement.

Why Testing the Final Finished Fabric Matters

Greige, dyed, and coated fabric represent different production stages. Heat, tension, resin application, and curing can change the result, so acceptable tear strength before coating does not verify the finished product.

For PU-coated ripstop, build the following checks into development and bulk approval:

  • Testing the base fabric during development when required

  • Testing again after the final coating process

  • Using the approved coating formulation for bulk

  • Recording key processing parameters

  • Taking the approval specimen from representative production

  • Repeating the required tests if the coating route changes

Our article on outdoor fabric testing explains why a passing material report does not replace evaluation of the complete garment.

What Buyers Should Put in a Ripstop Fabric Specification

A useful RFQ should contain more than “polyester ripstop with PU coating.”

Buyers should define:

  • Intended garment and use conditions

  • Fiber composition

  • Yarn denier

  • Weave and ripstop grid

  • Warp and weft density

  • Target GSM and tolerance

  • Usable width

  • Required hand feel

  • Coating type and coated side

  • Tear test method

  • Warp and weft tear requirements

  • Testing stage

  • Abrasion method, cycles and evaluation endpoint

  • AATCC 22 initial and after-wash requirements where applicable

  • Hydrostatic pressure method and target if waterproof performance is required

  • Color and colorfastness requirements

  • Sample approval procedure

  • Bulk testing and shipment-release conditions

If the buyer has only a garment sample or reference fabric, the specification can be developed through physical analysis and trial production. CC Textile supports fabric development from a reference sample, target construction or performance requirement.

The Cost of Discovering the Problem Too Late

A lower quote may reflect a lighter construction, different yarns, a lower-cost coating, or fewer tests. It may also reflect legitimate savings from production scale or sourcing. The price alone does not explain the difference.

Compare quotes that cover the same construction, finish, and testing responsibilities. A small saving on the fabric can be outweighed by:

  • Failed laboratory testing

  • Coating adjustments

  • Repeat sampling

  • Reprocessing costs

  • Delayed garment production

  • Missed shipment dates

  • Disputes over responsibility

Buyers should compare quotations against the same written specification. Our article explaining why fabric prices vary covers the costs that may be missing from an apparently similar offer.

Ripstop Fabric Approval Checklist

Before approving bulk PU-coated ripstop, the sourcing team should confirm:

  • Does the ripstop construction match the approved sample?

  • Are yarn denier, density, GSM and usable width within tolerance?

  • Was tear strength tested on the final coated fabric?

  • Are warp and weft requirements both stated?

  • Is the coating formulation suitable for the lightweight base fabric?

  • Are coating temperature and processing parameters controlled?

  • Is the abrasion requirement linked to a defined test method?

  • Is the AATCC 22 requirement separated from waterproof testing?

  • Has the garment factory checked sewability and seam construction?

  • Is written approval required before shipment?

Ripstop describes a reinforcement structure, not a guaranteed tear-strength level. In the 50D polyester project, the grid stayed the same; changes to the PU formulation, processing parameters, and temperature brought the finished fabric slightly above the required minimum.

Buyers with a ripstop sample, lightweight jacket concept or performance specification can contact CC Textile for construction and finishing evaluation.

For wider industry discussion about ripstop construction and fabric testing, visit Textile Alliance. Related fabric development updates are also shared through CC Textile on LinkedIn.

Frequently asked questions

What is ripstop fabric, and is it tear-proof?

Ripstop is a woven fabric with reinforcement yarns that form a grid. The grid can help limit tear propagation, but it does not prevent all tearing. Yarn strength, density, construction, finishing, and the test method determine the final result.

Can PU coating reduce the tear strength of ripstop fabric?

Yes, in some constructions. An unsuitable coating or processing route can make lightweight fabric too stiff or brittle. Test the final coated material instead of assuming how it will behave.

When should PU-coated ripstop be tested for tear strength?

Test the finished coated fabric because coating can change its mechanical behavior. Testing the base cloth as well can help identify where a change occurs during development.

Is an abrasion target of 16,000 cycles a complete specification?

No. Also specify the method, abrasive material, load, endpoint, and pass criteria. Cycle counts from different abrasion methods are not directly comparable.